Resolco® Insul-Phen Technical Data Sheet |
| PROPERTIES |
STANDARD |
Resolco |
US UNITS
|
| COLOR |
|
Tan
|
THERMAL CONDUCTIVITY
|
ASTM C-518
|
0.13 Btu-in./hr-ftsq DegF@75 DegF
|
NOMINAL DENSITY
|
ASTM D-1622
|
2.5 lb/ft cu.
|
TEMPERATURE LIMITS
|
|
-290DegF + 250DegF
|
SPECIFIC HEAT
|
|
0.45 Btu/lb.DegF
|
COMPREHENSIVE STRENGTH
-Parallel to rise
-Perpendicular to rise
|
ASTM D-1621
|
29 lb/in-sq
17.5 lb/in-cu
|
TENSILE STRENGTH
-Parallel to rise
-Perpendicular to rise
|
ASTM D-1623
|
35 lb/in-sq
26 lb/in-sq
|
SHEAR STRENGTH
-Perpendicular to rise
|
ASTM C-273
|
18 lb/in-sq
|
LINEAR EXPANSION COEFFICIENT
|
ASTM D-696
|
12E-06 inch/inch Deg F
|
THERMAL AND HUMID AGING
|
ASTM D-2126-87
-100°F for 7 days
-156°F for 7 days 100% RH
+267°F for 7 days
|
1" dim. 0.40 4" dim. 0.10
1" dim. 1.0 4" dim. 1.0
1"dim. 2.50 4" dim. 1.0
|
CLOSED CELL CONTENT
|
ASTM D-2856
|
>. 90%
|
WATER VAPOR PERMEABILITY
|
ASTM E-96
|
0.117 perm inch
|
WATER ABSORPTION
|
ASTM C-209
ASTM D-2842
|
0.5% by volume
0.10 lb/ft-sq
|
TUMBLING FRIABILITY
|
ASTM C-421
|
Abrasion loss less than 20%
|
CHLORIDE/FLUORIDE CONTENT
|
ASTM C-871
|
Meets the chemical requirements of ASTM C-795. NRC Regulatory Guide 1.36 and MIL-1-24244C with Amendment 1
|
STRESS CORROSION CRACKING ON AUSTENTIC STAINLESS STEEL
|
ASTM C-692
|
Meets the pre-production corrosion requirements of ASTM C-795 NRC Regulatory Guide 1.36 and MIL-I-24244C with Amendment 1
|
SURFACE BURNING CHARACTERISTICS
|
ASTM E-84
1" (25mm) thk, insulation only
|
Flame spread <25
Smoke developed <50
|
WEIGHT RETENTION
|
ASTM D-3014-74
|
85%
|
CRITICAL OXYGEN INDEX
|
ASTM D-2863
|
45%
|
| PUNKING |
BS 5946
|
Non punking
|
HOT SURFACE PERFORMANCE
|
ASTM C-411
|
No warping or joint opening.
No gassing or odor. Fully suited for use at operating temperatures up to and including 250DegF (120DegC)
|
|
|
|